Rigid PVC Molding Defects: How to Solve Splay, Blush, and Peel
Chapters
Welcome
0:0Few Words About Paul Mastro
1:34Identifying Splay, Blush, and Peel
2:8Molding Defect #1: Splay
3:10Molding Defect #2: Peel
4:12Molding Defect #3: Blush
5:5Troubleshooting Approach
6:24Start with Melt Temperature
7:39Step-by-Step Troubleshooting #1: Splay
9:27Step-by-Step Troubleshooting #2: Peel
13:11Step-by-Step Troubleshooting #3: Blush
14:24Conclusion
16:25
Paul Mastro
Sign-up and Track all your learning now!
Free Course Details
Who Should Watch this Video Tutorial:
This video tutorial suited for rigid PVC molders who only rely on past experience to solve routine molding issues.
Splay, blush & peel are very common rigid PVC molding defects. They look alike and each can have multiple specific causes… which mean as many potential solutions! Learn a systematic method and:
- Start well with a reliable defects identification: Splay vs. Blush vs. Peel
- Keep troubleshooting efforts minimal: pursue first high probability solutions
So, stop guessing what the solution might be... and lower your scrap rate!